摘要
Effects of minor Sc and Zr on the microstructure and mechanical properties of Al-4.6Cu-0.3Mg-0.6Ag alloys were investigated. The results indicate that Sc- and Zr-containing alloy as well as Sc-containing alloy could produce grain refinement effects. Both the alloys had lower tensile strength and hardness compared to Sc- and Zr-free alloy, mainly because solution heat treatment could not dissolve W (Al8.5-4Cu6.6-4Sc) phase, lowering the Cu concentration in the Al matrix. Insufficient Cu solute atoms in the Al matrix could not produce a large amount of Ω and θ′ strengthening precipitates to enhance the tensile strength and hardness following T7 heat treatment. However, the T7-treated Sc-containing alloy and the T7-treated Sc- and Zr-containing alloy have similar mechanical properties. Zirconium can partially replace expensive Sc to produce grain refinement effects on Al-Cu-Mg-Ag alloys.
原文 | ???core.languages.en_GB??? |
---|---|
頁(從 - 到) | 1165-1172 |
頁數 | 8 |
期刊 | Journal of Materials Engineering and Performance |
卷 | 24 |
發行號 | 3 |
DOIs | |
出版狀態 | 已出版 - 3月 2015 |