Atomic layer deposition of aluminum-doped zinc oxide films for the light harvesting enhancement of a nanostructured silicon solar cell

Sheng Hui Chen, Shih Hao Chan, Chun Ko Chen, Shao Ze Tseng, Chieh Hsiang Hsu, Wen Hao Cho

Research output: Contribution to journalArticlepeer-review